阻燃剂浓度对桉木胶合板胶合强度和润湿性的影响

Influence of Flame Retardant Concentration on Bonding Strength and Wettability of Eucalyptus Flame-retardant Plywood

  • 摘要: 采用单板浸渍和成板浸渍2种不同的阻燃处理方法制备桉木阻燃胶合板,并对其胶合强度和润湿性进行检测。结果表明:在相同浸渍时间和相同热压条件下,成板浸渍处理的胶合板胶合强度较高,胶合强度随着阻燃剂浓度变化不大;单板浸渍阻燃剂后制备的胶合板胶合强度较低,胶合强度随阻燃剂浓度的不同出现较大变化;阻燃处理提高了单板的润湿性,在阻燃剂浓度为5%~15%时,单板的润湿性随着阻燃剂浓度的提高而增大。

     

    Abstract: Eucalyptus flame-retardant plywood was made by 2 different flame retardant methods, i.e. veneer impregnation and board impregnation, and their bonding strength and wettability were measured. The results showed that plywood with board impregnation treatment had higher bonding strength than that treated with veneer impregnation. In case of board impregnation, bonding strength of plywood remained stable with the enlargement of flame retardant concentration, while for veneer impregnation, the bonding strength of plywood varied largely when the flame retardant concentration changed. Fire retarding treatment improved the wettability of veneers. In 5%-15% range of flame retardant concentration, wettability increased with the enlargement of flame retardant concentration.

     

/